Specialty Grinding and Polishing


Specialty Solutions
Specialty Grinding and Polishing
Coarse Polishing
Coarse polishing is the first polishing step after grinding and is typically done using diamond abrasive.
UltraPrep® Diamond Lapping Films
UltraPrep diamond lapping films are designed for applications where surface flatness and minimal deformation is critical. These lapping films are available in a wide range of sizes from 0.1µm to 30µm. Applications include microelectronic devices, wafers, ceramics, optical fibers, petrographic, and more.
FibrMet® Abrasive Discs
Abrasive® Powders
Abrasive powders are for fine grinding of cast iron and tin materials. Mixing is required with distilled water to achieve desired consistency.
Ordering
| UltraPrep Diamond Lapping Films (Qty 5) | ||
|---|---|---|
| UltraPrep Diamond Lapping Films are designed for various material applications including microelectronic devices, wafers, ceramics, optical fibers, petrographic, and other metallographic materials. Ideal for preparation applica- tions where surface flatness and minimal deformation are critical. | ||
| Micron | 8in [203mm] PSA Backed | 8in [203mm] Plain Backed |
| 0.1µm | 15-6791 | 15-6792 |
| 0.5µm | 15-6795 | 15-6796 |
| 1µm | 15-6801 | 15-6802 |
| 3µm | 15-6803 | 15-6804 |
| 6µm | 15-6806 | 15-6807 |
| 9µm | 15-6809 | 15-6810 |
| 15µm | 15-6815 | 15-6816 |
| 30µm | 15-6830 | 15-6831 |
| FibrMet Abrasive Discs (Qty 50) | |||
|---|---|---|---|
| FibrMet Abrasive Disc are PSA (polyester backed) films, approx. 0.1 mm thick, coated with an aluminum oxide abrasive. These discs can be used wet or dry and are most suitable for fine grinding and polishing application, such as optical fiber and microelectronics where resultant surface flatness is essential. | |||
| Micron | 4in [102mm] | 8in [203mm] | 12in [305mm] |
| 0.3μm | 69-3104 | 69-3174 | 69-3124 |
| 1μm | 69-3103 | 69-3173 | 69-3123 |
| 3μm | 69-3102 | 69-3172 | 69-3122 |
| 9μm | 69-3101 | 69-3171 | 69-3121 |
| 12μm | 69-3100 | 69-3170 | |
| Aluminum Oxide Powder | |
|---|---|
| Aluminum Oxide Powder is used for fine grinding on cast iron, tin, or cloth-covered platens. They are mixed with distilled water to the desired consistency. | |
| Part Number | Description |
| 406603030080 | 3µm 5lb [2.3kg] |
| 406605050080 | 5µm 5lb [2.3kg] |
Find Your Solutions
Full Lab
Metallography Solutions
Do you want to improve your process? Reach out for one-on-one help from our applications experts.

View all Products in the Buehler Product Catalog

Select a method by material

Search Buehler's Safety Data Sheets

Browse and search Buehler's product literature
Europe | EN