Wilson® Rockwell® 2000 Hardness Tester


The Rockwell 2000 Series hardness testing machines achieve the highest level of depth measurement accuracy and resolution available and as a result has the best GR&R performance in the industry. This machine is offered in two sizes ranging from 10 - 14 in of vertical testing capacity to accommodate varying sample sizes and is available in three different variations of Rockwell Regular, Superficial, or Twin hardness scales.

Industry-leading GR&R performance

  • Load cell force application ensure fast, precise, and reliable testing. Highly accurate "in-line" depth measuring scale

Ease of use

  • One button start – tester controls load application speed and dwell times
  • A flexible and user-friendly LCD control panel for method set up and configuration.

Flexible

  • Available in two sizes ranging from 10 - 14 in (254 – 356 mm) to accommodate varying sample sizes.
  • Available in three different variations: Regular, Superficial, or Twin hardness scales.
  • Large amount of accessories

Wilson® Rockwell® 2000 Hardness Tester
Wilson® Rockwell® 2000 Hardness Tester Specifications
  2002R & 2003R Regular 2002S & 2003S Superficial 2002T & 2003T Twin
Pre-load 10kgf 3kgf 3, 10kgf
Main-load 60, 100 150kgf 15, 30, 45kgf 15, 30, 45, 60, 100, 150kgf
Hardness scales HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRP, HRR, HRS, HRV, 15Y 15N, 30N, 45N, 15T, 30T, 45T, 5W, 30W, 45W, 15X, 30X, 45X, 30Y, 45Y HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRP, HRR, HRS, HRV, 15N, 30N, 45N, 15T, 30T, 45T, 15W, 30W, 45W, 15X, 30X, 45X, 15Y, 30Y, 45Y
Test load type Electronic closed-loop loadcell
Test cycle type Automatic, one button start
Vertical test capacity 2002 models 10in [254mm]; 2003 models 14in [356mm]
Horizontal test capacity 8.5in [216mm]
Indenters (optional) 120° Diamond cone, 1/16in, 1/8in, 1/4in, 1/2in Ball
Resolution 0.1 or 0.01 HR (adjustable)
Data-out RS232
Standards Compliant ASTM E18, B254, ISO 6508, JIS Z2245
Power 100, 120, 220 or 240VAC +/- 10%, 47-63Hz

Part Number Description Quick Quote
WH2002R Size - 2 Regular scale main unit Quick Quote
WH2002S Size - 2 Superficial scale main unit Quick Quote
WH2002T Size - 2 Twin scale main unit (Regular & Superficial) Quick Quote
WH2003R Size - 3 Regular scale main unit Quick Quote
WH2003S Size - 3 Regular scale main unit Quick Quote
WH2003T Size - 3 Regular scale main unit Quick Quote

Accessories & Related Products for the Wilson® Rockwell® 2000 Hardness Tester


Wilson® Rockwell® 2000 Hardness Tester
Watch the Wilson® Rockwell® 2000 Hardness Tester Video